weight = actual thickness × actual width × length (in) ÷ 1,728 × density (lb/ft³)
Densities are approximate for kiln-dried lumber near 12% moisture, which is how framing lumber is usually sold. Freshly pressure-treated lumber can be much heavier because it is wet from treatment; it gets lighter as it dries.
Weight of an 8 ft board (lb)
| Size | SPF (~27 lb/ft³) | Douglas fir (~34) | Southern pine (~36) | Treated, wet (~50) |
|---|---|---|---|---|
| 2×4 | 7.9 | 9.9 | 10.5 | 14.6 |
| 2×6 | 12.4 | 15.6 | 16.5 | 22.9 |
| 2×8 | 16.3 | 20.5 | 21.8 | 30.2 |
| 2×10 | 20.8 | 26.2 | 27.8 | 38.5 |
| 2×12 | 25.3 | 31.9 | 33.8 | 46.9 |
| 4×4 | 18.4 | 23.1 | 24.5 | 34 |
| 6×6 | 45.4 | 57.1 | 60.5 | 84 |
Approximate values; actual weight varies with moisture and growth.